Using busbar electroplating and subsequent drawing processes: effectively controls the consistency of the zinc plating thickness, improves electro-machining performance, increases processing precision, and improves cutting efficiency by more than 10%.
Mechanical Properties
Name | Grade | Copper Content (%) | Tensile Strength | Elongation | Conductivity |
Brass Wire | CuZn40 | 58.5-60.5 | 900-1000N/mm² | 1.5% | 22%IACS |
CuZn37 | 60.5-63.5 | 900-1000N/mm² | 1.5% | 22%IACS | |
CuZn35 | 63.5-68.0 | 900-1000N/mm² | 1.5% | 22%IACS | |
Galvanized Wire | -- | -- | 900-1000N/mm² | 1.5% | 22%IACS |
Gamma Wire | -- | -- | 900-1000N/mm² | 1.5% | 22%IACS |
Supply Method
Coil/Diameter (mm/inch)/Weight (KG) | |||||||
Coil | 0.07/0.003 | 0.10/0.004 | 0.15/0.006 | 0.20/0.008 | 0.25/0.010 | 0.30/0.012 | 0.33/0.014 |
P3 | 1.0/1.5 | 1.5/3.0 | 3.0 | 3.0 | 3.0 | 3.0 | -- |
P5 | -- | -- | 6.0 | 6.0 | 6.0 | 6.0 | 6.0 |
P10 | -- | -- | 10.0 | 10.0 | 10.0 | 10.0 | 10.0 |
P15 | -- | -- | -- | 20.0 | 20.0 | 20.0 | 20.0 |
K125 | 1.0/1.5 | 1.5/3.0 | 3.5 | 3.5 | 3.5 | 3.5 | -- |
K160 | -- | -- | 8.0 | 8.0 | 8.0 | 8.0 | 8.0 |
K200 | -- | -- | -- | 16.0 | 16.0 | 16.0 | 16.0 |
K250 | -- | -- | -- | -- | 25.0 | 25.0 | 25.0 |
Packaging
Quantity per Carton | |
Coil | Number of Spools |
P3 | 4 |
P5 | 4 |
P10 | 2 |
P15 | 1 |
K125 | 4 |
K160 | 2 |
K200 | 1 |
K250 | 1 |
Application Fields
● Precision Machining ● Mold Making ● Aerospace Industry ● Automotive Industry
Related Downloads
Kainan Group Product Brochure
Download
Message
We can recommend suitable products for you according to your needs. Please fill in the following form, and we will contact you in time!