The unique surface cleaning solution formula and online cleaning process improve the cleanliness of the electrode wire surface, reduce the powder shedding rate during the electrode wire processing, and improve the surface finish of the workpiece.
Mechanical Properties
Name | Grade | Copper Content (%) | Tensile Strength | Elongation | Conductivity |
Brass Wire | CuZn40 | 58.5-60.5 | 900-1000N/mm² | 1.5% | 22%IACS |
CuZn37 | 60.5-63.5 | 900-1000N/mm² | 1.5% | 22%IACS | |
CuZn35 | 63.5-68.0 | 900-1000N/mm² | 1.5% | 22%IACS | |
Galvanized Wire | -- | -- | 900-1000N/mm² | 1.5% | 22%IACS |
Gamma Wire | -- | -- | 900-1000N/mm² | 1.5% | 22%IACS |
Supply Method
Coil/Diameter (mm/inch)/Weight (KG) | |||||||
Coil | 0.07/0.003 | 0.10/0.004 | 0.15/0.006 | 0.20/0.008 | 0.25/0.010 | 0.30/0.012 | 0.33/0.014 |
P3 | 1.0/1.5 | 1.5/3.0 | 3.0 | 3.0 | 3.0 | 3.0 | -- |
P5 | -- | -- | 6.0 | 6.0 | 6.0 | 6.0 | 6.0 |
P10 | -- | -- | 10.0 | 10.0 | 10.0 | 10.0 | 10.0 |
P15 | -- | -- | -- | 20.0 | 20.0 | 20.0 | 20.0 |
K125 | 1.0/1.5 | 1.5/3.0 | 3.5 | 3.5 | 3.5 | 3.5 | -- |
K160 | -- | -- | 8.0 | 8.0 | 8.0 | 8.0 | 8.0 |
K200 | -- | -- | -- | 16.0 | 16.0 | 16.0 | 16.0 |
K250 | -- | -- | -- | -- | 25.0 | 25.0 | 25.0 |
Packaging
Quantity per Carton | |
Coil | Number of Spools |
P3 | 4 |
P5 | 4 |
P10 | 2 |
P15 | 1 |
K125 | 4 |
K160 | 2 |
K200 | 1 |
K250 | 1 |
Application Areas
● Precision Machining ● Mold Making ● Aerospace Industry ● Automotive Industry